JMV400 Aluminum & Metal Composite Panels LLDPE
Acid-Anhydride-Modified LLDPE Bonding Resin for ACP (High Flow) JMV400
High-flow variant of JMV300 with enhanced melt fluidity for improved processing efficiency.
Product Overview
JMV400 is the high-flow variant of JMV300, also an acid-anhydride-modified LLDPE resin. With MFI of 4.1 g/10min, it offers significantly improved melt flow for ACP production lines prioritizing throughput.
Typical Technical Properties
HuntHumber JMV400| Property | Test Method | Typical Value | Unit |
|---|---|---|---|
| Base Resin | - | LLDPE | - |
| Density | ASTM D792 / ISO 1183 | 0.930 | g/cm³ |
| Melt Flow Rate (MFR) | ASTM D1238 / ISO 1133 | 4.1 | g/10 min |
| Melting Point (Tm) | ASTM D3418 / ISO 3146 | 125 | °C |
| Vicat Softening Point | ASTM D1525 / ISO 306 | 100 | °C |
| MAH Grafting Content | Internal titration | Low (< 0.2 wt%) | - |
| Bonds To / Targets | - | Al, GS, PE | - |
| Recommended Processing / Use | - | Blown film / Coex coating | - |
Typical laboratory values for grade selection reference, not specification limits.
Typical Applications
- Aluminum Composite Panel (ACP) adhesive layer
- Thermal lamination adhesive film
- Metal-to-polyolefin bonding
- Heat-resistant composite panels
Performance Advantages
- High flow: MFI 4.1 g/10min for efficient extrusion processing
- Anhydride-modified bonding: Strong metal-to-polyolefin adhesion
- Improved processing efficiency: Supports efficient extrusion processing on production lines prioritizing throughput
- LLDPE mechanical advantages: Heat resistance and mechanical strength combined
Processing notes
- Maximum processing temperature: 250°C
- Optimize temperature and screw speed based on line speed and film gauge